Homogeneity and Penetration Depth of Atmospheric Pressure Plasma Polymerization onto Electrospun Nanofibrous Mats

Investor logo

Warning

This publication doesn't include Institute of Computer Science. It includes Central European Institute of Technology. Official publication website can be found on muni.cz.
Authors

MICHLÍČEK Miroslav MANAKHOV Anton DVOŘÁKOVÁ Eva ZAJÍČKOVÁ Lenka

Year of publication 2019
Type Article in Periodical
Magazine / Source Applied Surface Science
MU Faculty or unit

Central European Institute of Technology

Citation
Web https://www.sciencedirect.com/science/article/pii/S0169433218332240
Doi http://dx.doi.org/10.1016/j.apsusc.2018.11.148
Keywords Plasma polymers; Discharges; Carboxyl groups; Electrospun nanofibers; Penetration depth; Thin film characterization
Description This work investigates for the first time the penetration depth, nanoscopic homogeneity and conformality of the plasma polymerization onto an electrospun nanofibrous mat. The study is carried out on the model example of atmospheric pressure plasma co-polymerization of anhydride-rich films onto polycaprolactone mats that can find a significant practical applications, for example in tissue engineering and regenerative medicine. Since the surface-to-volume ratio of nanofibrous mats is enormous and the structure of mats resembles extracellular matrix the successful plasma coating of each whole fiber and understanding the penetration of the polymerization into the mat structure are extremely important. The films with reactive anhydride groups were prepared by co-polymerization of maleic anhydride and acetylene using dielectric barrier discharge. The studies were accompanied by the quantification of anhydride groups directly on the PCL electrospun mat using the chemical derivatization with trifluoroethylamine and X-ray photoelectron spectroscopy. The nanoscopic homogeneity and conformality of the anhydride plasma polymer coating on the front side and backside of the nanofibrous mat, 30-40 mu m in thickness, did not differ according to the dynamic SIMS mapping. The films containing approximately 6 anhydride groups per 100 carbon atoms coated homogeneously the nanofibers deeper in the PCL mat. The characteristic penetration depth of the deposition was estimated as 46 +/- 5 mu m.